MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade

Material Notes: Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences in compatibility. To minimize viscosity changes in hot melt blends during processing, Elvax® 40W also contains butylated hydroxytoluene(BHT). Elvax®40W is supplied in pellet form and to prevent the pellets from blocking, low levels of an amide wax have been added to the polymer.

Typical Applications:

  • Laminating adhesives for a variety of substrates including plastics and films. This grade provides the extended open time often needed in industrial assembly
  • Lacquers for wood, metal, metal foils, paper, and films
  • Fabric and decal coatings
  • Heat-seal coatings for backing card stock used in blister packaging
  • Wood primers and sealers. Combinations of Elvax® 40W and nitrocellulose form the basis for wood sealers offering toughness and good intercoat adhesion
      Elvax® 40W is also suggested for use as a modifier in:
  • Elastomer-based hot melt and hot melt pressure-sensitive adhesion formulations
  • Natural and synthetic elastomers to improve resistance to ozone cracking
  • Caulks and sealants, including those based on asphalt
  • Asphalt road repairing compositions for resurfacing, patching, and crack sealing to improve low temperature flexibility, strength properties, and adhesion
  • Traffic paint formulations
  • Solvent-based and wax-based inks

Information provided by DuPont.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.965 g/ccASTM D1505
Viscosity Measurement 0.70
@Temperature 30.0 °C
Inherent, 0.25 g/100mL toluene
Vinyl Acetate Content 40 %DuPont Method
Melt Index of Compound 52 g/10 minASTM D1238, modified
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 4010 seconds, Shore A-2; ASTM D2240
Tensile Strength at Break 4.80 - 6.20 MPaSamples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D1708
Elongation at Break 1000 - 1300 %Samples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D1708
Tensile Modulus 0.00300 GPaSamples die cut from pressed films, gage dimensions 2.23cm x 0.47cm x 0.13cm, crosshead speed 2in/min; ASTM D638
 
Thermal PropertiesOriginal ValueComments
Ring & Ball Softening Point 104 °CASTM E28
 
Descriptive Properties
Antioxidant550 ppmBHT
OdorSlight
Residual VA Monomer, wt%<0.3
Vinyl Acetate Content40 wt.%DuPont Method

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Arkema EVATANE® 42-60 Copolymer Ethylene - Vinyl Acetate
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Arkema EVATANE® 40-55 Copolymer Ethylene - Vinyl Acetate
ExxonMobil Escorene™ UL 05540EH2 Ethylene Vinyl Acetate Copolymer (European Grade)
Dow Elvax® 40L-03 Ethylene-Vinyl Acetate Copolymer Resin

PDUPM120 / 33787

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.