MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK PRIEX® 20093 Maleic Anhydride Grafted PP homopolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Functionalised polypropylene to be used as compatibiliser for polymer blends or coupling agent for glass fiber, wood flour, natural fibers, multilayer films, aluminum foils, or mineral filled polypropylene.

Examples: Compatibilising short-and long glass fibers and PP applications such as automotive applications (instrument panel carrier, front-end, door modules, etc.) and Wood filled polymer composites.

Mode of action and advantages: PRIEX® 20093 is a polypropylene, grafted with a high content of maleic anhydride. The grafted maleic anhydride introduces polarity to the polymer achieving compatibility between polyolefins and more polar polymers like EVOH.

Advantages: Excellent mechanical properties, good cost / performance; Ultra low smell, low VOC and emissions; Excellent coupling agent for short and long glass filled polyolefins providing enhanced physical, mechanical and thermal properties; Excellent coupling agent for natural fiber reinforced polymer composites or wood flour reinforced polymer composites; Free flowing pellets; and Safe and easy handling.

Food contact: PRIEX® 20093 composition meets the requirements of Commission Directive 2002/72/EC and further amendments.

Former Addcomp product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-3
Viscosity Test 70 - 80 cm³/gIntrinsic viscosity; ISO 1628
Oxidative Induction Time (OIT) >= 20 min
@Temperature 190 °C
ISO 11357-6
Melt Flow 9.0 - 13 g/10 min
@Load 0.325 kg,
Temperature 190 °C
die 8/2; ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 165 °CISO 11357-3
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 280 °C
 
Descriptive Properties
AppearanceWhite or slightly yellow granules
Free Aleic Anhydride<250 mg/kgSolvay method
Grafted Maleic Anhydride0.17-0.21%Solvay method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK PRIEX® 25097 Maleic Anhydride Grafted PP random copolymer
BYK PRIEX® 20095 Maleic Anhydride Grafted PP homopolymer
BYK PRIEX® 20070 Maleic Anhydride Grafted PP homopolymer
BYK PRIEX® 15005 Maleic Anhydride modified LDPE
BYK PRIEX® 12031 Maleic Anhydride Grafted HDPE

PPADDC02 / 130314

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.