MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Thermoset™ MD-200 Electrically Conductive Die-Attach Adhesive
Categories: Polymer; Adhesive

Material Notes: This is a system with the versatility to fit a wide variety of production and performance needs. The working life allows sufficient time for short production interruption. It can be initially cured at room temperature in 24 hours. Suitable for applications in which the part will not tolerate elevated temperatures. The cure schedule can also be shortened to 40 minutes by oven curing.
Intended Use: Chip-on-board die-attach.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.75 g/cc
Viscosity 70000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D2240
Shear Strength 1500 psi
@Temperature 25.0 °C
Die; 0.05" x 0.05" IC; Chatillon Force Gauge Model DPP-25
 1500 psi
@Temperature 25.0 °C
Tensile; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.09 W/m-K
Glass Transition Temp, Tg 105 °CPerkin-Elmer DSC-2
 
Processing PropertiesOriginal ValueComments
Cure Time 40.0 min
@Temperature 95.0 °C
Complete
 180 min
@Temperature 65.0 °C
Complete
 1440 min
@Temperature 25.0 °C
Initial
 4320 - 7200 min
@Temperature 25.0 °C
Complete
Pot Life 60 min
@Temperature 25.0 °C
Shelf Life 6.00 Month
@Temperature 25.0 °C
Resin
 12.0 Month
@Temperature 25.0 °C
Hardener
 
Descriptive Properties
AppearanceSilver
Mix Ratio100:10by weight
 100:35by volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Thermoset™ MT-125 Thermally Conductive Adhesive
Lord Adhesives Thermoset™ MD-130 Electrically Insulating Die-Attach Adhesive
Epoxy Technology EPO-TEK® T905BN-3 Thermally Conductive Epoxy
Dow TC-5688 Thermally Conductive Compound
Dow TC-5022 Thermally Conductive Compound

PLORD042 / 86050

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.