MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Plastcom SLOVALEN PC 93 T 15 1/M PP, 15% mineral filling, UV stability  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler; Polypropylene with 20% Talc Filler

Material Notes: Features

Modified PP for injection molding with the content of 15% mineral filling, uv stabilized. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shrinkage. General application in all industry branches. Very good scratch and odor resistant.

Packaging, transport, stocking

The product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The product requires storage in closed-up, dry places protected against sun and thermal radiation.

Information Provided by Plastcom spol. s r.o.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Linear Mold Shrinkage 0.0193 cm/cm
Linear Mold Shrinkage, Transverse 0.0188 cm/cm
Melt Flow 20 g/10 min
@Load 0.325 kg,
Temperature 270 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.0 MPa
Elongation at Break 8.0 %
Tensile Modulus 2300 MPa
Flexural Strength 44.0 MPa
Flexural Modulus 2200 MPa
Charpy Impact Unnotched 68.0 kJ/m²
@Temperature -20.0 °C
 75.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -20.0 °C
 16.0 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 250 °C
Mold Temperature 40.0 - 50.0 °C
Drying Temperature 80.0 °C
Dry Time 4 hour
Injection Pressure 70.0 - 120 MPa

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Daplen™ MD206U Polypropylene Compound 20% Mineral Filled
Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled
Borealis Daplen™ KSR65T20 Polypropylene Compound 20% Mineral Filled
Borealis Daplen™ KSX65T20 Polypropylene Compound 20% Mineral Filled

PPLACO285 / 120909

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.