MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Tra-Con Tra-Bond K5NA Ablative Thermal Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND K5NA is a three-part, ablative and thermally insulating epoxy compound used in aerospace applications. This smooth, trowellable system is specified by NASA for the Space Shuttle`s solid rocket boosters for close-out and patching of the boosters` thermal protection systems. It is also used for void filling and protecting wires, tubing and other surface protrusions on hypersonic re-entry bodies, nose cones and aircraft engines. TRA-BOND K5NA is impact resistant which makes it an excellent choice for lightweight casting requirements. TRA-BOND K5NA develops strong bonds to most all substrates. It maintains excellent dimensional stability over a wide temperature range and provides protection to weathering, ozone and moisture.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.600 g/cc0.600 g/ccMixed
Solids Content 100 %100 %Reactive Solids Content
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 1515
Tensile Strength, Yield 0.689 MPa100 psi
Izod Impact, Notched 53.4 J/cm100 ft-lb/in
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.100 W/m-K0.694 BTU-in/hr-ft²-°F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 240 min
@Temperature 65.0 °C
2.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 30 min30 min
 
Descriptive Properties
Color Light Brown
Heat of Combustion BTU/lbm 1450
Mix Ratio, parts by weight100/75/25Resin/Hardener/Part C
Thermal Diffusivity ft2/hr 0.0031

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tra-Con Tra-Bond K6 Ablative Thermal Epoxy Compound
Momentive Performance Materials RTV5812 One-Component, Modified Alkoxy Adhesive Sealant, White
General Plastics LAST-A-FOAM® R-9320 Thermal Isolation Blocks
General Plastics LAST-A-FOAM® FR-7108 Polyurethane Foam
General Plastics LAST-A-FOAM® FR-7104 Polyurethane Foam

PTRAC301 / 71229

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.