MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
RTP Company RTP 201H HS  Nylon 6/6 - High Impact (PA 6/6 HI) Glass Fiber 10% - Heat Stable - High Impact  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Glass Reinforced, Impact Grade

Material Notes: Glass Fiber 10% - Heat Stable - High Impact

Comments:

  • High Impact
  • Glass Fiber
  • Heat Stabilized

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.


Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccASTM D792
Filler Content 10 %
Water Absorption 0.90 %24 hours at 23°C; ASTM D570
Linear Mold Shrinkage 0.0070 cm/cm
@Thickness 3.17 mm
ASTM D955
 0.012 cm/cm
@Thickness 6.35 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 113ASTM D785
Tensile Strength, Ultimate 13000 psiASTM D638
Elongation at Break 4.0 %ASTM D638
Modulus of Elasticity 650 ksiASTM D638
Flexural Yield Strength 20000 psiASTM D790
Flexural Modulus 520 ksiASTM D790
Compressive Yield Strength 9000 psiASTM D695
Izod Impact, Notched 3.50 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Izod Impact, Unnotched 22.0 ft-lb/in
@Thickness 3.17 mm
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Constant 3.55
@Frequency 1e+6 Hz
Dry; ASTM D150
Dielectric Strength 500 V/milS/T; ASTM D149
Dissipation Factor 0.020
@Frequency 1e+6 Hz
Dry; ASTM D150
Arc Resistance 90 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 26.0 µin/in-°F
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 2.80 BTU-in/hr-ft²-°FThrough-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 487 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 450 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
Per testing by RTP Company; ASTM D635
 
Processing PropertiesOriginal ValueComments
Processing Temperature 525 - 560 °F
Mold Temperature 150 - 225 °F
Injection Pressure 15000 - 18000 psi
 
Descriptive Properties
ColorNatural/Black

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PR3849 / 63151

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.