MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

5251-H22 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95251; Aluminium 5251; AA5251-H22; Al5251-H22
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.69 g/cc0.0972 lb/inĀ³AA; Typical
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 6565
Tensile Strength, Ultimate 210 MPa30500 psi
Tensile Strength, Yield 165 MPa23900 psi0.2% offset
Elongation at Break 14 %14 %
Shear Strength 125 MPa18100 psi
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 95.4 - 98.2 %95.4 - 98.2 %As remainder
Chromium, Cr <= 0.15 %<= 0.15 %
Copper, Cu <= 0.15 %<= 0.15 %
Iron, Fe <= 0.50 %<= 0.50 %
Magnesium, Mg 1.7 - 2.4 %1.7 - 2.4 %
Manganese, Mn 0.10 - 0.50 %0.10 - 0.50 %
Other, each <= 0.050 %<= 0.050 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.40 %<= 0.40 %
Titanium, Ti <= 0.15 %<= 0.15 %
Zinc, Zn <= 0.15 %<= 0.15 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
5251-O Aluminum
Aluminum 6082-T6
5251-H24 Aluminum
5251-H26 Aluminum
Aluminum 5052-H32

MA5251H22 / 130357

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.