MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Arla ATECH® 3000 ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: ATECH® is a series of sheets based on ABS which is a raw material with very high impact-strength. ABS also has impressive thermal qualities and is easy to thermoform and fabricate. ATECH® 3000 is a super high impact ABS with a semigloss surface that thermoforms quickly and effectively.
Also Available In: ATECH® 3003 has extra UV stabilizers added to improve weather resistance; ATECH® 3000 FA is a food compliant product version; Stripes for identification purpose; Dual coloring to optimize to specific needs.
Recycling: The total recycling concept (TRC) covers all types of sheets to provide cost savings. Off-cuts from the sheets can be used in production of new sheets by co-extruding virgin material as the top layer. Care is taken that all quality requirements are met.

Benefits: Easy to thermoform; High impact strength; Good thermal qualities

Application: In general where a high impact strength material is needed like machine covers, high demanding general purpose & indoor applications.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ISO 1183
Linear Mold Shrinkage 0.0060 - 0.0070 cm/cm0.0060 - 0.0070 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 77.0 MPa11200 psiISO 2039
Tensile Strength at Break 25.0 MPa3630 psiISO 527-2
Tensile Strength 31.0 MPa4500 psiISO 527-2
Tensile Strength, Yield 31.0 MPa4500 psiISO 527-2
Elongation at Break >= 2.0 %>= 2.0 %at Tensile strength; ISO 527-2
 >= 40 %>= 40 %ISO 527-2
Elongation at Yield >= 2.0 %>= 2.0 %ISO 527-2
Tensile Modulus 1.60 GPa232 ksiISO 527-2
Flexural Strength 55.0 MPa7980 psiISO 178
Flexural Modulus 2.00 GPa290 ksiISO 178
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 13.0 kJ/m²
@Temperature -23.0 °C
6.19 ft-lb/in²
@Temperature -9.40 °F
ISO 180/A
 27.0 kJ/m²
@Temperature 23.0 °C
12.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched  1.00 J/cm²
@Temperature -40.0 °C
4.76 ft-lb/in²
@Temperature -40.0 °F
ISO 179-1/1eA
 1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179-1/1eA
 1.30 J/cm²
@Temperature -23.0 °C
6.19 ft-lb/in²
@Temperature -9.40 °F
ISO 179-1/1eA
 2.60 J/cm²
@Temperature 23.0 °C
12.4 ft-lb/in²
@Temperature 73.4 °F
ISO 179-1/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear 65.0 µm/m-°C
@Temperature 20.0 - 70.0 °C
36.1 µin/in-°F
@Temperature 68.0 - 158 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °FISO 75-2
Vicat Softening Point 96.0 °C205 °FB120; ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PARLA901 / 301079

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.