MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Clwyd Compounders IR Polyisoprene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: The synthetic equivalent to Natural Rubber is polyisoprene (IR) which can be produced by polymerization of 2-methyl-1,3-butadiene with Ziegler-Natta catalyst.

Typical applications: TIn applications where consistency and good processability is required, synthetic polyisoprene is often the better choice. Since the polymerization of isoprene is carried out under narrowly controlled conditions, there is very little variation of composition, structure, and resulting properties, whereas natural rubber contains naturally occurring impurities and the molecular weight varies with the growth conditions of the rubber tree. Both has a noticeable impact on the physical properties and processability of the rubber.

Advantages: In general, synthetic rubber has superior resistance to aging and weathering and is easier toprocess due to its lower viscosity. It is also often more compatible with other rubbers such as SBR and EPDM.

Disadvantages: Synthetic polyisoprene has lower strength than natural rubber but better low-temperature properties.

Information provided by CLWYD COMPOUNDERS LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 30 - 9530 - 95
Tensile Strength <= 23.0 MPa<= 3340 psi
Elongation at Break <= 600 %<= 600 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °FUpper continuous
Minimum Service Temperature, Air -70.0 °C-94.0 °Fnon-brittle
 -50.0 °C-58.0 °Fsealing applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCLWYD032 / 316049

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.