MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Emerald Performance Materials EPALLOY® 8240 Epoxy Phenol Novolac Resin
Categories: Polymer; Thermoset; Epoxy; Epoxy, Novolac, Molding Compound

Material Notes: Phenol Novolac Epoxy Resins:
  • Excellent chemical resistance
  • High-functionality, cross-link density & Tg
Description / Use: Lowest viscosity unmodified epoxy novolac available. Lower in viscosity than standard Bis-A resin. EPALLOY 8240 is preferred for secondary containment tank linings and industrial flooring.

Information provided by Emerald Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 6000 - 7100 cP
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0
 
Descriptive Properties
Average Epoxy Functionality2.35
EEW164-176 g/eq
HCC<0.1%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Emerald Performance Materials EPALLOY® 8250 Epoxy Phenol Novolac Resin
Cookson Group Plaskon® 3100 Novolac Epoxy Molding Compound
Cookson Group Plaskon® 440 Mineral Filled Novolac Epoxy Molding Compound
Kaneka Kane Ace MX-215 Epoxidized Novolac Resin
Lotte Advanced Materials Radianz® Engineered Quartz Stone

PEMERA803 / 209631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.