MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® A 145 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Water-reducible, hydroxyfunctional polyacrylic dispersion. In combination with aliphatic polyisocyanates to formulate aqueous two-component clear- and topcoats for vehicle repair applications, heavy transport finishing and industrial coating. In combination with amino resins or blocked polyisocyanates for waterborne, one-component, industrial baking coatings.

Properties / Applications:
General: Bayhydrol® A 145 is a hydroxyfunctional polyacrylic dispersion which can be thinned with water to application viscosity. Bayhydrol® A 145 has good pigment wetting properties and high shear stability. Bead mills have proved suitable as grinding equipment. Only pigments and extenders with a minimal water-soluble content should be used. Given the many pigments and extenders available, compatibility testing should always be carried out. Leveling and substrate wetting can be optimized by adding Byk® 380 or Byk® 348, for example. Byk® 011 has proved to be a suitable antifoam. Application and formulation equipment can be cleaned with water, alkaline cleaning agents or isopropanol.
Two-component industrial coatings: Bayhydrol® A 145 combined with aliphatic polyisocyanates yields high-gloss topcoats which can be dried at room temperature or force-dried, e.g. at 80 °C. The cured paint films are hard and flexible with good single-coat adhesion and good resistance to solvents and water. When properly formulated, e.g. in combination with Bayhydur® 3100 in an NCO/OH ratio of 1.5 : 1, the pot life is approximately 3 hours. The formulated coating should have a pH between 7.8 and 8.3. When mixing Bayhydur® or Desmodur® into the mill base, a thickener must be added to ensure a high shear effect. The addition of approx. 0.3 % Acrysol® RM 8 (calculated on the solid binder) has proved suitable for formulations based on Bayhydrol® A 145.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/ccDIN EN ISO 2811-2
Volatiles 53 - 57 %1g/1h/125 °C/convection oven; DIN EN ISO 3251
pH 7.5 - 8.5thinned 1 : 4 with demineralized water; DIN ISO 976
Viscosity 400 - 1500 cPD = 41,28 s-1; DIN EN ISO 3219/A.3
 
Chemical PropertiesOriginal ValueComments
Acid Value 7.0 - 13[mg KOH/g]; DIN EN ISO 2114
 
Thermal PropertiesOriginal ValueComments
Flash Point 45.0 °CDIN EN ISO 1523
 
Descriptive Properties
Content3.3%OH

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Bayhydrol® A 2457 Polyurethane Coating
Dow Bynel® 30E753 Anhydride Modified Ethylene Vinyl Acetate
Covestro Bayhydur® XP 2451/1 Polyurethane Coating
Dymax 3073 Solvent-Free Plastic Adhesive
ExxonMobil LD 145.PX Packaging Resin

PCOVEST0147 / 201930

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.