MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Turbo Oil 2197
Categories: Fluid

Material Notes: Product Description: Eastman™ Turbo Oil 2197 is designed to exceed the demand of current and future turbine engines. With over 400 million hours of in-flight experience, it is by far the most widely used HTS fleet oil in the world. Eastman™ Turbo Oil 2197 is manufactured in our own facility so you can rely on consistently high quality wherever you are in the world. Eastman™ Turbo Oil 2197 is AS5780 HPC / MIL-PRF-23699 HTS class, 5 cSt turbine oil for the most thermally demanding engine and accessory applications.

Application/Uses:

  • Aeroderivative engine
  • Aviation
  • Engine Accessories
  • Engines
Key Attributes:
  • 5 cSt High Thermal Stability synthetic lubricant
  • High temperature cleanliness
  • Outstanding Oxidative, Thermal and Hydrolytic stability

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9968 g/ccASTM D1298
Kinematic Viscosity 5.28 cSt
@Temperature 98.9 °C
ASTM D445
 26.98 cSt
@Temperature 37.8 °C
ASTM D445
 12539 cSt
@Temperature -40.0 °C,
Time 2100 sec
ASTM D2532
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.36[mg KOH/g]; SAE ARP5088
 
Thermal PropertiesOriginal ValueComments
Pour Point -57.0 °CASTM D97
Flash Point 262 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM5265 / 222459

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.