Product Description: Grilamid L 20 EC is an electrically conductive, medium viscosity injection molding product, based on Polyamid 12 (PA12). Grilamid L 20 EC is heat stabilized, easy to process with good mold release characteristics. The inherent color of this material is black. The main characteristics of this product are: - Electrically conductive
- Heat stability
- Good chemical resistance
- Good resistance to oil
- High surface quality
- Good dimensional stability
- Easy to process
- Low density, low weight
Application examples: Grilamid L 20 EC is suitable for injection molding parts in electro/electronic applications: Antistatic housings, covers and functional parts.Information provided by EMS Grivory. |