MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ineos H12G-01 Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade; Polypropylene, Molded

Material Notes: Grade H12G-01 is a general purpose homopolymer. This material meets the requirements of the US Food and Drug Administration as specified in 21 CFR 177.1520 for use in food-contact applications for food type Categories I through IX of Table 1, under conditions of use A through H of Table 2 in Title 21 CFR, Part 176.170(c).
    Applications:
  • General Purpose Injection and Extrusion
  • Housewares
  • Rigid Packaging
  • Caps & Closures
  • Film and Sheet

    Information provided by Ineos Olefins & Polymers USA

Key Words: General purpose
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.911 g/ccASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103Injection Molded; ASTM D785
Hardness, Shore D 76ASTM D2240
Tensile Strength at Break 2400 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 5200 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 110 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 9.4 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 244000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.590 ft-lb/inInjection Molded; ASTM D256
Izod Impact, Notched (ISO) 1.48 ft-lb/in²Area, Injection Molded; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 216 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 307 °FASTM D1525
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessExtrusion
 Injection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ineos N12N-00 Polypropylene Impact Copolymer
Ineos H36G-01 Polypropylene Homopolymer
Ineos H38G-02 Polypropylene Homopolymer
Ineos R35C-02 Polypropylene Random Copolymer
Americhem Engineered Compounds ColorRx™ PP1-2002AF Food Grade Polypropylene Homopolymer

PINEOS911 / 130370

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.