MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Matexcel MCP-002 Spherical Activated Carbon
Categories: Other Engineering Material

Material Notes: Because of its high purity, low dust, spherical shape, low pressure loss and super purification ability, spherical activated carbon has been used in the fields of adsorption materials for purification room filters in the semiconductor industry, gas treatment of electronic devices, etc. Activated carbon adsorption treatment is a branch of water treatment. With the strengthening of water pollution and related management measures, the demand for activated carbon is also increasing.

Morphology: Powder

Key Words: Synonyms: Spherical Activated Carbon
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
Product overviewParticle size: 1mm±0.2 Moisture: 8.9% Ash: 0.1% Strength 99.3 Packing density: 0.61 g/ml PH:5.51 Iodine value: 1340 Pore size: ~10nm Specific surface area: 1273 (m2/g), Carbon tetrachloride value CCI4:74

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMXCK2019 / 300650

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.