MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ITW Plexus Plexus™ MA590 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.

All purpose, long open time product and bond lines up to 1" thick

Information provided by Illinois Tool Works.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.959 g/cc0.0346 lb/in³Mixed
Viscosity 175000 - 220000 cP175000 - 220000 cPA
 175000 - 220000 cP175000 - 220000 cPB
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 17.2 - 20.7 MPa2500 - 3000 psi
Elongation at Break 150 - 180 %150 - 180 %
Tensile Modulus 0.621 - 0.758 GPa90.0 - 110 ksi
Shear Strength 11.0 - 13.8 MPa1600 - 2000 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
Flash Point 10.6 °C51.0 °FTCC
 
Processing PropertiesMetricEnglishComments
Pot Life 90 - 105 min90 - 105 min
 
Descriptive Properties
ColorBlack
Fixture Time1100 psi in 4 hours
 800 psi in 3 hours
Gap FillingMax 1 in
Mix Ratio1:1By volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM9013 / 53322

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.