MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Armacell Monarch® F-06905 (Gray) NBR/PVC Foam
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes:

Information provided by Armacell®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 - 15.0 lb/ft³ASTM D1056
Water Absorption <= 5.0 %ASTM D1056
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore OO 80 - 90ASTM D2240
Tensile Strength 200 psiASTM D412, Die A
Elongation at Break 150 %ASTM D412, Die A
Compressive Strength 20.0 - 32.0 psi
@Strain 25 %
ASTM D1056
Resilience 5.0[%]; ASTM D2632
Tear Strength >= 24.0 pliDie C; ASTM D624
Compression Set <= 25 %ASTM D1056
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 160 °FContinuous; ASTM D746
 220 °FIntermittent; ASTM D746
Minimum Service Temperature, Air -20.0 °FASTM D746
 
Descriptive Properties
Accelerated Aging±30%Change in Compression Deflection, 7 days at 70°C, ASTM D1056
ColorGray
FlammabilityFMVSS302Pass
 HF-1Passable, but not UL listed
Fluid Immersion<50%Weight Change, 7 days at 23°C, Fuel B, ASTM D1056

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATG s.r.l. ACM Polyacrylic Rubber
Armacell Monarch® F-02003 (Black) Neoprene Based Rubber Foam
Versalis Europrene® N OZO 5033 NBR-PVC blend
Silikony Polskie Polastosil M-99 Silicone Rubber
Seals Eastern 7189 Ethylene-Propylene Rubber

PARMD107 / 186718

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.