MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Johnson Matthey Silver-flo™ 43 Cadmium Free Silver Brazing Filler Metal
Categories: Metal; Nonferrous Metal; Precious Metal; Solder/Braze Alloy

Material Notes: Silver-flo™ 43 is a cadmium free silver brazing alloy. It is not a commonly used or specified alloy. However, it was originally developed by Johnson Matthey in research to find a low silver content filler metal alloy that is resistant to dezincification in marine environments. As such this alloy is suitable for seawater applications, and is still used in some naval or marine work where written specifications call for it.

Silver-flo™ 43 has a brazing temperature that is above the annealing or stress relieving temperature of many copper-nickel alloys. Consequently Silver-flo™ 43 has been used on cupro-nickel and high nickel content copper alloys where stress cracking / intergranular penetration may otherwise be a problem.

Silver-flo™ 43 has a relatively long melting range, is not free flowing and will fill joint gaps at brazing temperature of between 0.075-0.2mm. It can therefore be used for filling joints that cannot be tightly controlled.

This filler metal can be used to join all the common engineering materials (excluding aluminum) – such as copper, copper alloys (including, brasses, bronzes, gun metal, nickel silvers, aluminum bronze, copper nickel) and steel (including, mild, carbon, tool steel, stainless steels and low alloy steel).

Information provided by Johnson Matthey Metal Joining

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Melting Point 690 - 775 °C1270 - 1430 °F
Solidus 690 °C1270 °F
Liquidus 775 °C1430 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 20 %20 %
Silver, Ag 43 %43 %
Zinc, Zn 37 %37 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Johnson Matthey Pallabraze™ 1179 Precious Metal Brazing Filler Metal
Johnson Matthey Argo-braze 49LM Trifoil Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze 49H Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Argo-braze 40N Silver Brazing Alloy for Tungsten Carbide Brazing
Johnson Matthey Active-braze™ No. 2 Silver Brazing Filler Metal

NJMMJ9764 / 186165

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.