Isopar-E solutions of MMAO-7 are used as co-catalysts in the polymerization of olefins and other monomers via single-site catalysts. CAS number: 206451-54-9 EINECS/ELINCS No: 931-025-3 Applications: Isopar E solutions of MMAO-7 are used as cocatalysts in polymerization of olefins and other monomers via single-site catalysts. Information provided by Nouryon |