MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Invista 1101 PET Copolymer Packaging Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Carboxyl end groups: <30 meg/kg.
Diethylene glycol content: <1.8 wt%.
Acetaldehyde content: <2.0 ppm.
Fines 0.1% through 28 mesh as manufactured.
Moisture content <0.1% as manufactured.
Chip size <1.8±0.3mm avg. dia. flat side.
Crystallinity >50%.

1101 PET is a copolymer packaging resin with a nominal intrinsic viscosity of 0.84 dl/g. 1101 resin has excellent melt and crystallization properties, offering easy processibility in injection molding and stretch-blow molding.

Packaging made from this resin has excellent clarity and is noted for its dimensional stability, which prevents shrinkage and expansion of the container. It conforms to FDA Regulation 177.1630 for food contact and is widely used for single-serve beverage bottles, small liquor bottles, and other custom containers. Containers made from PET are light weight, have excellent clarity, are recyclable, and are shatterproof.

Information supplied by the manufacturer.

The Invista PET product line has been acquired by Indorama.

Key Words: Excellent melt and crystallization properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.830 g/cc
Density >= 1.39 g/ccWI No. 300 test
Viscosity Measurement 0.81 - 0.85Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 246 °CWI No. 72A test
 
Descriptive Properties
processBlow Molding
 Injection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Invista 2201 PET Copolymer Packaging Resin
Eastman Aqua 18696 PET
Eastman CM01 PET
Eastman Eastar GN078 Copolyester, Natural
Invista 1102 PET Copolymer Packaging Resin

PKO000 / 48897

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.