MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Thermal Ceramics Cerablanket AC2 Blanket
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Thermal Ceramics Cerablanket AC2 insulating blanket provides enhanced performance over the acoustical properties of Cerablanket AC1. Cerablanket AC2 has been engineered to combine the benefits of improved acoustical performance with high mechanical strength. This combination enables Cerablanket AC2 to perform in the most demanding applications. Avalible thicknesses- 1, 1.5, 2 in. Avalible widths- 24, 48 in.

Features:Excellent sound absorption, Thermal stability, Low heat storage, Superior handling strength, Flexible and resilient, Immune to thermal shock, Highly resistant to vibration, Excellent thermal insulating performance.

Applications:HRSG silencers, Mufflers, Sound Walls.

Information provided by Thermal Ceramics

Data has not been recently verified. Please contact manufacturer for current information.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0480 g/ccAvailable in multiple densities
 0.0640 g/ccAvailable in multiple densities
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 6.00 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 2150 °F
 
Component Elements PropertiesOriginal ValueComments
Al2O3 45 - 47 %
Other 0.00 - 1.0 %
SiO2 53 - 55 %
 
Descriptive Properties
Leachable chlorides, ppm<10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Thermal Ceramics Cerablanket Blanket

CTHERM005 / 2325

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.