MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt NORSODYNE® S 81302 AL Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Orthophthalic

Appearance: Grey - Light -Veiled

Main resin characteristics: Fire retardant properties, Good transparence, Light stabilized, Medium reactivity, Preaccelerated, Very good glass wet-out, Very long shelf life

Main applications: Transparent and corrugated sheets

Molding information: Continuous laminating, Hand lay up and Spray up

Curing cycle: 16 h at 80°C + 2 h at 120°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³
Solids Content 64 - 72 %64 - 72 %MT-CU001C
Brookfield Viscosity 390 - 430 cP390 - 430 cPsp 2 rpm 50; MT-CUT23V
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 33.0 MPa4790 psiISO 527
Elongation at Break 1.0 %1.0 %ISO 527
Tensile Modulus 4.08 GPa592 ksiISO 527
Flexural Strength 50.0 MPa7250 psiISO 178
Flexural Modulus 4.074 GPa590.9 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 75.5 °C168 °FISO 75 -2A
 
Processing PropertiesMetricEnglishComments
Cure Time 3.25 - 4.25 min
@Temperature 85.0 °C
0.0542 - 0.0708 hour
@Temperature 185 °F
Reactivity at 85°C + peroxides; MT-CU026R
Gel Time 2.00 - 2.67 min
@Temperature 85.0 °C
2.00 - 2.67 min
@Temperature 185 °F
Reactivity at 85°C + peroxides; MT-CU026R
Shelf Life 6.00 Month6.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm208 - 223°CMT-CU026R; Reactivity at 85°C + peroxides

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9368 / 231963

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.