TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, electronic, appliance, automotive and optical industries. Characteristics: - Medium viscosity
- 30% glass fiber
Applications: - 3025R type reinforced by glass fiber (short fiber). particularly suitable for injection molding where especially good dimensional stability is required
All information provided by Samyang |