MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy
Categories: Polymer; Thermoplastic; Ionomer; Nylon (Polyamide PA)

Material Notes: Description

Formion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.
Application

Formion® FI 232H is targeted for non painted, mold-in-color, exterior or interior appearance applications.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.09 g/cc1.09 g/ccISO 1183/1
Linear Mold Shrinkage  0.0010 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0060 in/in
@Thickness 0.126 in
72 hr; ISO 294
 0.0011 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0011 - 0.0070 in/in
@Thickness 0.126 in
aged 48 hrs at 121°C; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 38.0 MPa5510 psiISO 527
Elongation at Break 325 %325 %ISO 527
Flexural Modulus 1.70 GPa247 ksiTangent; ISO 178
Izod Impact, Notched (ISO) 65.0 kJ/m²30.9 ft-lb/in²pb; ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
@Thickness 3.20 mm
216 °F
@Thickness 0.126 in
ISO 75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman FORMION™ FI 234 20% Mineral Reinforced Ionomer / Nylon Alloy
A. Schulman FORMION™ FI 200 Non-Reinforced, Injection Molding Grade Ionomer / Nylon Alloy
Dow Surlyn® 2601B Sodium Ionomer
Dow Surlyn® 6320 Magnesium Ionomer
Dow Surlyn® 8528 Sodium Ionomer

PASHU028 / 24992

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.