MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Carpenter Vega® Alloy Tool Steel (Air-Tough) (AISI A6)
Categories: Metal; Ferrous Metal; Tool Steel

Material Notes: Vega die steel combines the deep hardening and minimum size change characteristics of air-hardening steels with the simplicity of low temperature heat treatment possible in many oil-hardening steels. It is available as a DeCarb-Free product. DCF bars have been cold finished in the mill, eliminating the need for bar bark removal.

Applications: Large blanking dies, Large forming dies, Trimming dies, Notching dies, Feed fingers, Heavy duty punches, Coining dies, Retaining rings, Rim rolls, Master hubs, Shear blades, Precision tools, Spindles, Bending tools, Mandrels, Stripper plates, Plastic molds

Information provided by Carpenter Technology Corporation.

Vega® is a registered trademark of Carpenter Technology Corporation.

Key Words: UNS T30106
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 7.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 48 - 49Tempered at 1200°F
 61 - 62As hardened
Tensile Strength, Ultimate 2350 MPawhen tempered at 350°F
Tensile Strength, Yield 2100 MPawhen tempered at 350°F
Elongation at Break 1.0 %when tempered at 350°F
Reduction of Area 2.0 %when tempered at 350°F
Modulus of Elasticity 200 GPa
Izod Impact Unnotched 155 Jwhen tempered at 350°F
Charpy Impact 1.00 JV-Notch, when tempered at 350°F
Charpy Impact, Unnotched 130 J
@Treatment Temp. 177 °C
tempered at 350°F
Abrasion 73.8loss in mm3, As-Hardened; ASTM G65
 130.7loss in mm3, Tempered at 1100°F; ASTM G65
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.8 µm/m-°C
@Temperature 20.0 - 100 °C
 13.7 µm/m-°C
@Temperature 20.0 - 400 °C
 14.7 µm/m-°C
@Temperature 20.0 - 700 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.70 %
Chromium, Cr 1.0 %
Iron, Fe 94.65 %As Balance
Manganese, Mn 2.0 %
Molybdenum, Mo 1.35 %
Silicon, Si 0.30 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type S14800 Stainless Steel condition CH900, 72.5% cold reduction
AISI Grade 18Ni (350) Maraging Steel, Aged, at RT, tested transverse, sheet 6 mm thick
EOS MS1 Maraging Steel Sintered on EOSINT M 270
TIMET 6-6-2 Titanium Alloy (Ti-6Al-6V-2Sn), Solution Treated and Aged
Hexcel® HexPly® EH04 Epoxy Resin System, T600 Fiber

NCARN19 / 15858

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.