MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Tra-Con Tra-Bond 2106T Fast Cure Thixotropic Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: TRA-BOND 2106T is an exceptional epoxy formulation recommended for lower temperature or wet industrial bonding applications where FAST CURING is required. This versatile two-part epoxy system contains no solvents, mixes easily at room temperature, and is suitable for high performance structural bonding applications where the combination of very fast room temperature curing coupled with low shrinkage and excellent mechanical and electrical properties is needed. It develops strong, tough bonds to metals, plastics, glass and glass fabrics, hardboards and forestry products, ceramics, rubber, masonry materials, and other construction materials. When fully cured, TRA-BOND 2106T is an excellent electrical insulator, and provides superior resistance to vapors and gases, water, galvanic action, petroleum fuels, salt solutions, and many other organic and inorganic compounds. TRA-BOND 2106T develops significant properties 1 hour after mixing. However, an extended cure of 4-6 hours at 25°C is required for fully matured bonds. Note: TRA-BOND 2106T develops a high exotherm. Use immediately after mixing. The exothermic reaction begins within 2 minutes after initiating the mixing step, so have everything ready before removing the BIPAX clamp.

Information provided by Tra-Con Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/ccMixed
Solids Content 100 %Reactive Solids Content
Viscosity 3600 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 25After 10 min
 67After 30 min
 72After 60 min
Adhesive Bond Strength 200 psiLap shear, alum to alum
Izod Impact, Notched 1.90 ft-lb/in
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+11 ohm-cm
Dielectric Constant 4.8
@Frequency 1000 Hz
Dielectric Strength 410 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 µm/m-°C
@Temperature 20.0 °C
Maximum Service Temperature, Air 115 °C
 150 °CIntermittent
Minimum Service Temperature, Air -60.0 °C
 -60.0 °CIntermittent
Glass Transition Temp, Tg 25.0 °CUltimate Tg
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 hour
@Temperature 65.0 °C
 4.00 - 6.00 hour
@Temperature 25.0 °C
Pot Life 5.0 min
 
Descriptive Properties
Color Hazy, Light Straw
Mix Ratio, parts by weight110/93Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Valley Adhesives EM-500 High Temperature Application Glue Stick
Momentive Performance Materials RTV6445 White Adhesive Sealant, Non-Corrosive High Strength Paste

PTRAC010 / 70938

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.