MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Huntsman IROGRAN® PS455-200 TPU-Polyester
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Introduction: IROGRAN PS455-200 is a polyester based thermoplastic polyurethane intended for extrusion applications. IROGRAN PS455-200 is part of the HUNTSMAN film and sheet product range and offers a specially designed, flexible material with a broad processing window particularly suitable for film and sheet, textile laminations, and compounding.

Performance Features:

  • FDA grade (21 CFR 175.105, 177.2600)
  • Soft
  • High elongation
  • Tough
  • Good low temperature properties
  • Wide processing window
Applications:
  • Textile lamination
  • Compounding

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³Injection molded parts; ASTM D792
Melt Index of Compound 8.0 g/10 min
@Load 2.16 kg,
Temperature 177 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 351 °F
MVR, [cm3/10 min]
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878Injection molded parts; ASTM D2240
Tensile Strength at Break 42.0 MPa6090 psi0.025" extruded film; DIN 53504
Elongation at Break 700 %700 %0.025" extruded film; DIN 53504
100% Modulus 2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
0.025" extruded film; DIN 53504
300% Modulus 5.00 MPa
@Strain 300 %
725 psi
@Strain 300 %
0.025" extruded film; DIN 53504
Rebound 50 %50 %Bayshore; ASTM D2632
Tear Strength 66.6 kN/m380 pli0.025" extruded film; ASTM D624
Abrasion 5050mm3, Injection molded; DIN 53516
Compression Set  40 %
@Temperature 22.8 °C,
Time 252000 sec
40 %
@Temperature 73.0 °F,
Time 70.0 hour
Injection molded; ASTM D395
 90 %
@Temperature 70.0 °C,
Time 86400 sec
90 %
@Temperature 158 °F,
Time 24.0 hour
Injection molded; ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 110 - 130 °C230 - 266 °F0.025" extruded film,
 
Processing PropertiesMetricEnglishComments
Feed Temperature 140 °C284 °FExtrusion
Middle Barrel Temperature 150 °C302 °FExtrusion
Adapter Temperature 150 °C302 °FExtrusion
Die Temperature 150 °C302 °FExtrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Huntsman IROGRAN® PS 455-204 TPU-Polyester
Huntsman IROGRAN® PS 455-215 TPU-Polyester
Huntsman IROGRAN® PS442-202 TPU-Polyester
Huntsman IROGRAN® PS 370-202 TPU-Polyester
Huntsman IROGRAN® A 85 P 4666 Ether-Based TPU-For Cable Industry

PHUQ110 / 159483

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.