MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polymer Resources PPX-SF1 Modified-PPO, Structural Foam Grade, Flame Retardant, Easy Flow
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, Heat Resistant

Material Notes: Modified-Polyphenylene Oxide, Structural Foam Grade, Easy Flow

Features: • Flame Retardant • Bromine Free • Chlorine Free • Self Extinguishing
Process: Foam Molding
Notes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.

Information provided by Polymer Resources Corporation.

Key Words: UL E113219; Polyphenylene Ether + PS
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/ccASTM D792
Linear Mold Shrinkage 0.0060 - 0.0090 cm/cmASTM D955
Melt Flow 25 - 50 g/10 min
@Load 11.6 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM D785
Tensile Strength at Break 9000 psiASTM D638
Tensile Strength, Yield 9200 psiASTM D638
Flexural Strength 12000 psiASTM D790
Flexural Modulus 460 ksiASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Temperature 22.8 °C
ASTM D256
Gardner Impact 150 in-lbASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 220 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 210 °FASTM D648
UL RTI, Electrical 149 °F
@Thickness 3.00 mm
UL 746
 149 °F
@Thickness 3.81 mm
UL 746
UL RTI, Mechanical with Impact 149 °F
@Thickness 3.00 mm
UL 746
 149 °F
@Thickness 3.81 mm
UL 746
UL RTI, Mechanical without Impact 149 °F
@Thickness 3.00 mm
UL 746
 149 °F
@Thickness 3.81 mm
UL 746
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0 - 5VA
@Thickness 3.80 mm
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 450 - 500 °F
Middle Barrel Temperature 520 - 580 °F
Front Barrel Temperature 520 - 580 °F
Melt Temperature 500 - 550 °F
Mold Temperature 100 - 180 °F
Drying Temperature 160 - 180 °F
Dry Time 3.00 - 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polymer Resources PPX-FR1 Modified-PPO, V-0 Flame Retardant
Mitsubishi Iupiace® LN30 m-Polyphenylene Ether (m-PPE)
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced
Shuman 211 Flame Retardant Polyphenylene Ether Copolymer Alloy
Mitsubishi Iupiace® LN60 m-Polyphenylene Ether (m-PPE)

PPOLYQ240 / 160764

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.