Telcar TL-8451G is a general purpose thermoplastic elastomer designed for electrical applications requiring flexibility over a wide temperature range. It is a medium durometer grade that is UV stabilized and RoHS compliant. This grade is suitable for injection molding and extrusion. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Features: General Purpose; Good Colorability; Good Flexibility; Halogen Free; High Elasticity; High Elongation; High Tensile Strength; Medium Flow; Ozone Resistant; Sunlight Resistant (720 hrs); UV Resistant; Weather Resistant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Insulation; Terminal Cable Jacketing; Underground Power Cable; Wire & Cable Applications; Wire Jacketing RoHS Compliant:RoHS Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |