MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
LATI Larpeek 10 G/15 PEEK, 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Glass Fiber Filled

Material Notes: Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.40 g/cc
Linear Mold Shrinkage, Flow 0.0040 - 0.0065 cm/cm
Linear Mold Shrinkage, Transverse 0.0070 - 0.010 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPa
@Temperature 150 °C
 90.0 MPa
@Temperature 120 °C
 110 MPa
@Temperature 90.0 °C
 125 MPa
@Temperature 60.0 °C
 135 MPa
@Temperature 23.0 °C
Elongation at Break 2.8 %
@Temperature 23.0 °C
 3.1 %
@Temperature 60.0 °C
 3.4 %
@Temperature 90.0 °C
 3.8 %
@Temperature 120 °C
 4.5 %
@Temperature 150 °C
Elongation at Yield 3.0 %
@Temperature 90.0 °C
 3.0 %
@Temperature 120 °C
 3.5 %
@Temperature 150 °C
Tensile Modulus 5100 MPa
@Temperature 150 °C
 5500 MPa
@Temperature 120 °C
 5700 MPa
@Temperature 90.0 °C
 6100 MPa
@Temperature 60.0 °C
 6300 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 40.0 kJ/m²
@Temperature -20.0 °C
 45.0 kJ/m²
@Temperature 23.0 °C
Charpy Impact, Notched 3.00 kJ/m²
@Temperature -20.0 °C
 4.00 kJ/m²
@Temperature 23.0 °C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 220 °C
Deflection Temperature at 0.46 MPa (66 psi) 290 °C
Deflection Temperature at 1.8 MPa (264 psi) 285 °C
Vicat Softening Point >= 300 °C
@Load 5.00 kg
Flammability, UL94 V-1
@Thickness 0.750 mm
 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 370 - 400 °C
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Latilub 88/10-15T G/30 PEEK, 30% Glass Fiber Reinforced, PTFE Filled
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced
LATI Larpeek 10 G/30 PEEK, 30% Glass Fiber Reinforced
RTP Company RTP 2202 HF  Polyetheretherketone (PEEK) Glass Fiber 15% - High Flow

PLATH9635 / 177331

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.