MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Lion Stereon™ SR8983 IP Styrene-butadiene
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Styrene Butadiene Rubber

Material Notes: Stereon™SR8983 is a solution polymerized linear styrene-butadiene multi-block thermoplastic elastomer. This material has been designed as a graftable rubber modifier that is reacted with bromine and processed into a clean, white powder. The brominated Stereon™SR8983 is then combined with polystyrene to produce a flame retardant foam insulation used in building and home construction.

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.890 g/cc0.890 g/cc
Volatiles <= 3.0 %<= 3.0 %ASTM D5668
Molecular Weight 125 - 155 g/mol125 - 155 g/molASTM D5296
 
Chemical PropertiesMetricEnglishComments
Styrene Content 31 - 35 %31 - 35 %Bound; ASTM D2702
 
Descriptive Properties
Content<0.01%Toluene Insolubles
 <1.2 %Polydispersity, ASTM D5296
 >79%Vinyl, ASTM D2702

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLION082 / 317991

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.