MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Ineos L12G-00 PP Impact Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; SAN Polymer; Styrene Acrylonitrile (SAN), Molded

Material Notes: Product Description: L12G-00 is medium melt flow rate, nucleate impact copolymer polypropylene for injection molding and compounding applications. It is especially formulated for high impact resistance, high flexural modulus and excellent gloss. Applications include automotive, consumer products, housewares and compounding.
Availability: North America
Additive: Nucleating Agent
Features: Food Contact Acceptable; High Gloss; High Impact Resistance; Impact Copolymer; Medium Flow; Nucleated
Uses: Automotive Applications; Compounding; Consumer Applications; Household Goods
Agency Rating: EC 1907/2006 (REACH); FDA 21 CFR 177.1520
RoHS Compliance: Contact Manufacture
Forms: Pellets
Processing Method: Compounding; Injection Molding

Information provided by INEOS Olefins & Polymers USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ASTM D792
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 8888ASTM D785
Tensile Strength at Break 18.1 MPa2620 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 25.8 MPa3740 psi2.0 in/min; ASTM D638
Elongation at Break 120 %120 %2.0 in/min; ASTM D638
Elongation at Yield 6.0 %6.0 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 1260 MPa183000 psiASTM D790A
Izod Impact, Notched  0.641 J/cm
@Temperature -20.0 °C
1.20 ft-lb/in
@Temperature -4.00 °F
ASTM D256
 1.92 J/cm
@Temperature 22.8 °C
3.60 ft-lb/in
@Temperature 73.0 °F
ASTM D256
Izod Impact, Notched (ISO)  6.01 kJ/m²
@Temperature -20.0 °C
2.86 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 18.9 kJ/m²
@Temperature 22.8 °C
8.99 ft-lb/in²
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C215 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 52.8 °C127 °FUnannealed; ASTM D648
Vicat Softening Point 148 °C299 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 74 %74 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINEOSA036 / 268272

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.