MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® ETFE
Categories: Polymer; Thermoplastic; Fluoropolymer; ETFE/ECTFE

Material Notes: A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and electrical properties comparable to typical fluoropolymer, such as PTFE, PFA and FEP and also is more progressive than ECTFE or PVdF with its improved mechanical strength and very easy moldability.

Information provided by Asahi Glass Company, Inc.

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 10.0 MPa
@Temperature 170 °C
 20.0 MPa
@Temperature 130 °C
 30.0 MPa
@Temperature 95.0 °C
 40.0 MPa
@Temperature 60.0 °C
Elongation at Break 400 %
@Treatment Temp. 20.0 °C
 500 %
@Treatment Temp. 45.0 °C
 500 %
@Treatment Temp. 185 °C
 600 %
@Treatment Temp. 155 °C
 600 %
@Treatment Temp. 75.0 °C
 800 %
@Treatment Temp. 120 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 41.8 - 50.2 J/g
Specific Heat Capacity 1.26 J/g-°C
Thermal Conductivity 0.1672 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 92.0 - 95.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 - 67.0 °CASTM D648
Flammability, UL94 V-0
Oxygen Index 32 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Zone 1 250 - 260 °CElectric wire covering
 270 °CFilm
 270 °CTube
Zone 2 270 - 290 °CElectric wire covering
 290 °CFilm
 290 °CTube
Zone 3 300 °CTube
 310 °CFilm
 330 - 340 °CElectric wire covering
Die Temperature 310 °CTube
 315 °CFilm
 350 - 360 °CElectric wire covering
 
Descriptive Properties
Fragility Temperature-125°CASTM D764

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carpenter Custom 630 (17-Cr-4Ni) Precipitation Hardening Stainless Steel, Condition H 1100 (Heated 593°C)
Iron Thermocouple Wire Type J - Standard
Constantan Thermocouple Wire
AGC Fluon® ETFE C-88AXM White Pigmentation
CENTROPLAST CENTROLEN PE-HD Polyethylene high density

PAGCX025 / 191134

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.