MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Paratherm Corporation Paratherm™ HR™ Heat Transfer Fluid
Categories: Fluid

Material Notes: Paratherm HR™ Heat Transfer Fluid is an alkylated-aromatic based heat transfer fluid formulated for closed loop liquid phase heating to 650°F in fired heaters and 675°F in waste heat recovery and full convection heaters.

Applications

  • Gas processing
  • Chemical processes
  • Waste oil recovery
  • Biodiesel production
  • Plastic processing

Information Provided by Paratherm Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 43.0 lb/ft³
@Temperature 371 °C
 46.0 lb/ft³
@Temperature 316 °C
 48.0 lb/ft³
@Temperature 260 °C
 51.0 lb/ft³
@Temperature 204 °C
 54.0 lb/ft³
@Temperature 149 °C
 56.0 lb/ft³
@Temperature 93.3 °C
 59.0 lb/ft³
@Temperature 37.8 °C
 62.0 lb/ft³
@Temperature -17.8 °C
Viscosity 0.32 cP
@Temperature 371 °C
 0.34 cP
@Temperature 357 °C
 0.36 cP
@Temperature 343 °C
 0.38 cP
@Temperature 329 °C
 0.41 cP
@Temperature 316 °C
 0.44 cP
@Temperature 302 °C
 0.47 cP
@Temperature 288 °C
 0.50 cP
@Temperature 274 °C
 0.54 cP
@Temperature 260 °C
 0.59 cP
@Temperature 246 °C
 0.64 cP
@Temperature 232 °C
 0.71 cP
@Temperature 218 °C
 0.78 cP
@Temperature 204 °C
 0.87 cP
@Temperature 191 °C
 0.98 cP
@Temperature 177 °C
 1.1 cP
@Temperature 163 °C
 1.3 cP
@Temperature 149 °C
 1.5 cP
@Temperature 135 °C
 1.8 cP
@Temperature 121 °C
 2.1 cP
@Temperature 107 °C
 2.6 cP
@Temperature 93.3 °C
 3.8 cP
@Temperature 79.4 °C
 5.1 cP
@Temperature 65.6 °C
 7.9 cP
@Temperature 51.7 °C
 12 cP
@Temperature 37.8 °C
 22 cP
@Temperature 23.9 °C
 52 cP
@Temperature 10.0 °C
 133 cP
@Temperature -3.89 °C
 546 cP
@Temperature -17.8 °C
Molecular Weight 240 g/molAverage
Vapor Pressure 0.00758 bar
@Temperature 163 °C
 0.0338 bar
@Temperature 204 °C
 0.117 bar
@Temperature 246 °C
 0.345 bar
@Temperature 288 °C
 0.896 bar
@Temperature 329 °C
 2.00 bar
@Temperature 371 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µin/in-°Fconverted from volume expansion
Specific Heat Capacity 0.440 BTU/lb-°F
@Temperature -17.8 °C
 0.470 BTU/lb-°F
@Temperature 37.8 °C
 0.500 BTU/lb-°F
@Temperature 93.3 °C
 0.530 BTU/lb-°F
@Temperature 149 °C
 0.560 BTU/lb-°F
@Temperature 204 °C
 0.590 BTU/lb-°F
@Temperature 260 °C
 0.620 BTU/lb-°F
@Temperature 316 °C
 0.650 BTU/lb-°F
@Temperature 371 °C
Thermal Conductivity 0.564 BTU-in/hr-ft²-°F
@Temperature 371 °C
 0.636 BTU-in/hr-ft²-°F
@Temperature 316 °C
 0.684 BTU-in/hr-ft²-°F
@Temperature 260 °C
 0.732 BTU-in/hr-ft²-°F
@Temperature 204 °C
 0.768 BTU-in/hr-ft²-°F
@Temperature 149 °C
 0.792 BTU-in/hr-ft²-°F
@Temperature 93.3 °C
 0.816 BTU-in/hr-ft²-°F
@Temperature -17.8 °C
 0.816 BTU-in/hr-ft²-°F
@Temperature 37.8 °C
Maximum Service Temperature, Air 650 °FFired Heaters
 675 °FAll Others
 700 °FFilm Temperature
Minimum Service Temperature, Air 13.0 °Fstart-up temp at 300 cPs
 77.0 °Foperating temp at 20 cPs
Pour Point <= -30.0 °FD97
Flash Point >= 320 °FClosed Cup (D93)
 >= 330 °FOpen Cup (D92)
 
Descriptive Properties
AppearanceAlmost Colorless
BaseAlkylated Aromatic
OdorSlight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Paratherm Corporation Paratherm™ HT Heat Transfer Fluid

WPAR04 / 104382

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.