MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Washington Penn PPH4CF1 Polypropylene, 10% Calcium Carbonate Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Calcium Carbonate (CaCO3) Filler

Material Notes: UV Stabilized; Injection molding grade.

Applications: High flow for thin wall parts requiring long-flow. Wash tubs.

Data provided by Washington Penn Plastic Co., Inc.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.09 g/ccASTM D792
Melt Flow 13 - 15 g/10 minCond L; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 31.0 MPaASTM D638
Flexural Yield Strength 31.0 MPaASTM D790
Flexural Modulus 1.60 GPaTangent; ASTM D790
Gardner Impact 11.0 JASTM D3029

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Washington Penn Medium Impact Copolymer 10% Talc Filled
Washington Penn Homopolymer Polypropylene 40% Glass Reinforced
Washington Penn Homopolymer Polypropylene 20% Talc Filled
Washington Penn Homopolymer Polypropylene 10% Talc Filled
Washington Penn High Modulus Polypropylene Homopolymer 40% Glass Filled

PWPP09 / 72792

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.