MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Henkel Turco 6849 Cleaner
Categories: Fluid; Solvent

Material Notes: Turco 6849 is a clear, aqueous alkaline degreaser formulated to remove shop soils, marking inks, COSMOLINE, grease and lube oils from ferrous and non-ferrous alloys. Offers both exceptional effectiveness and exceptional tank life. Replaces solvent-type vapor degreasing fluids with an effective aqueous cleaner. The costs and hazards normally associated with chlorinated solvent cleaning are thereby greatly reduced.
    Applications:
  • Alkaline Etch
  • Magnesium Phosphate Conversion Coatings
  • Zinc Phosphate Conversion Coatings
  • Boric Sulfuric Anodizing
  • Chromic Acid Anodizing
  • Phosphoric Acid Anodizing

Key Words: Aerospace Surface Treatment
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 55.0 - 70.0 °CImmersion
 
Descriptive Properties
ChemistryAlkalineWater-based
ConsistencyLiquid
FormConcentrated
SubstrateAluminum
 Ferrous
 Magnesium
 Stainless Steel
 Titanium

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Henkel Turco 4215 NC-LT Cleaner
Solvay Chemicals Hydrofluoric acid

PHENK880 / 146885

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.