Notes: Monprene CP-39972 CLR is a high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-39972 CLR is medium hardness grade that exhibits excellent sunlight resistance and is suitable for injection molding and extrusion. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Contact Clarity; Light Stabilized; Medium Flow; Medium Hardness; Low Density; Low Specific Gravity; Without Filler Uses: Consumer Applications; Gaskets; Handles; Tubing RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Preliminary data. Information provided by Teknor Apex |