MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eneos 0568 SBLTX
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Characteristics:
  • Low viscosity even though containing high molecular weight polymer
  • Low viscosity even though with high total solid content
  • High speed filming Capability
  • Easy and safe handling
Applications: Carpet, Fabric/Non Woven Fabric, Adhesive

ENEOS has acquired the elastomer product lines from JSR Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 %50 %
Water Absorption 113 %113 %
Particle Size 115 µm115 µm
pH 8.08.0
Brookfield Viscosity 220 cP220 cP60 rpm
Surface Tension 58 dynes/cm58 dynes/cm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 25.0 MPa3630 psi
Elongation at Break 1039 %1039 %
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -23.0 °C-9.40 °F
 
Descriptive Properties
10% weight reduction temperature374°C
Content (%)80Toluene GEL
Polymer TypeCarboxylated

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PJSRC8190 / 295506

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.