TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes. TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture. Tribological and mechanical properties: - Medium toughness
- Good lubrication properties
Advantages and applications: - Low friction coefficient
- Low wear of the counterpart
- Good transfer-film formation
- High electrical conductivity
- Suitable for pitch-bonded and resin-bonded brushes
- Fe-self lubricating engineering parts
- Fe-friction parts
- Copper/bronze bearings
- Copper friction parts copper clutch facings
Information provided by TIMCAL |