Application: Comonomer in paint resins and plastics. Appearance: Clear, colorless to yellowish liquid. Odor: Slightly ester-like CAS: 29964-84-9 Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale. |