MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Celanese Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Impact Grade

Material Notes: Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation, making this a material ideally suited to parts that are subjected to medium shock loads.

Key characteristics:

  • Low temperature impact resistance
  • High elongation, allowing snap fitting in dry-as-molded state
  • Good overall mechanical performance
  • Easy processing
  • Excellent surface finish

Information provided by NILIT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ASTM D792, ISO 1183
Water Absorption 2.5 %2.5 %23°C, 24h in H2O; sim. ISO 62
Water Absorption at Saturation 9.0 %9.0 %sim. ISO 62
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inEuronil
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inEuronil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 70.0 MPa10200 psiISO 527, ASTM D638
Elongation at Yield >= 100 %>= 100 %ISO 527, ASTM D638
Flexural Yield Strength 100 MPa14500 psiISO 178, ASTM D790
Flexural Modulus 2.50 GPa363 ksiISO 178, ASTM D790
Izod Impact, Notched (ISO)  5.00 kJ/m²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 180/1A
 11.0 kJ/m²
@Temperature 23.0 °C
5.23 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched NBNBISO 179
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179
 0.550 J/cm²
@Temperature -30.0 °C
2.62 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 18.0 kV/mm
@Thickness 2.00 mm
457 kV/in
@Thickness 0.0787 in
ASTM D149
Comparative Tracking Index  550 V
@Thickness 3.20 mm
550 V
@Thickness 0.126 in
Sol. B; IEC 112, UL 746A
 600 V
@Thickness 3.20 mm
600 V
@Thickness 0.126 in
Sol. A; IEC 112, UL 746A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 85.0 °C185 °F20,000 hr; IEC 216
Deflection Temperature at 0.46 MPa (66 psi) 175 °C347 °FISO 75, ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C149 °FISO 75, ASTM D648
Vicat Softening Point 185 °C365 °F49 N; ISO 306, ASTM D1525
 212 °C414 °F9.8 N; ISO 306, ASTM D1525
Flammability, UL94  HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
Glow Wire Flammability Index  650 °C
@Thickness 0.800 mm
1200 °F
@Thickness 0.0315 in
IEC 694-2-12
 650 °C
@Thickness 3.20 mm
1200 °F
@Thickness 0.126 in
IEC 694-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 240 - 270 °C464 - 518 °F
Zone 1 230 - 260 °C446 - 500 °Fhopper
Zone 2 230 - 260 °C446 - 500 °F
Zone 3 240 - 270 °C464 - 518 °F
Zone 4 240 - 270 °C464 - 518 °F
Melt Temperature 240 - 280 °C464 - 536 °FDo not melt above 300°C
Mold Temperature 60.0 - 80.0 °C140 - 176 °F80°C is Preferred
Drying Temperature 80.0 - 85.0 °C176 - 185 °F
Dry Time 4 hour4 hour
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi
 
Descriptive Properties
Clamping Forcein tons, 0.7 times the projected surface area in cm2
Heat Resistance - Ball TestOKat 125°C, IEC 309
 OKat 165°C, IEC 309
Holding Pressure90 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit Nilamid B3N Unfilled, Nucleated PA6
BASF Ultramid® 8254 HS BK-102 PA6 (Dry)
EMS-Grivory Grilon® BRZ 347 W PA6
Clariant PA233 Nylon 6, Improved Processability, Easily Colorable, Toughened
Celanese Zytel® MT409AHS BK010 PA66-I

PLBN45 / 50434

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.