ERISYS GE Series glycidyl ether modifiers are low molecular weight epoxy functional products based on alcohols, glycols and phenols. The product line covers a broad range of TSCA approved modifiers from monofunctional to multifunctional materials. Classified at right. Description / Use: C12-C14 Aliphatic Glycidyl Ether. Natural alcohol based. Used in flooring, aggregate bonding and adhesives. Information provided by Emerald Performance Materials. |