MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lanxess LEWATIT® S 5528 Anion Exchange Resin
Categories: Polymer; Thermoset

Material Notes: Lewatit® S 5528 is a food grade, macroporous, strongly basic anion exchange resin (type I) based on a crosslinked polyacrylate. It is bead-shaped and has a special bead size distribution for use in the following processes:
  • Co-current system
  • Counter-current systems (Lewatit WS system/fluidized bed)
  • Counter-current systems (Lewatit VWS system/compound fluidized bed)
In its chloride form, the Lewatit S 5528 is suitable for the decolorization of:
  • syrups from sugar production, especially cane sugar
  • solutions of organic products e.g. glycerin, amino acids
The macroporous structure and balanced resin matrix of Lewatit S 5528 facilitate the kinetics of adsorption and desorption. Substances adsorbed, e.g. high-molecular hydrophilic anionic organic substances and colorants from sugar solutions, can be desorbed easily be regeneration with a neutral or alkaline sodium chloride solution. Lewatit S 5528 is therefore highly recommended for use wherever complete and rapid removal of a relatively high concentration of organic substances is required. A use in combination with other Lewatit adsorber resins such as Lewatit S 6368 allows simultaneous fine polishing. When using Lewatit S 5528 to treat potable water and the aqueous solutions listed above, special care should be given to the initial cycles of the new resin.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.720 g/cc0.0260 lb/in³
Density 1.08 g/cc0.0390 lb/in³
Bead Size 0.400 - 1.60 mm0.0157 - 0.0630 in>90%
Storage Temperature -20.0 - 40.0 °C-4.00 - 104 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceWhite, opaque
pH Operating Range0 - 12

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANY8832 / 209224

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.