MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by elevated temperatures.

Information provided by Epoxyset Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.00 g/cc
Viscosity 1000 - 1600 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ASTM D2240
Shear Strength 12.0 MPa
Adhesive Bond Strength 1400 psiLap Shear Strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000500 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 62.0 µm/m-°C
Thermal Conductivity 1.60 W/m-K
Maximum Service Temperature, Air 150 °C
Minimum Service Temperature, Air -55.0 °C
Glass Transition Temp, Tg 65.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 hour
@Temperature 80.0 °C
 48.0 hour
@Temperature 25.0 °C
Pot Life 240 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Atom Adhesives AA-DUCT 916 Epoxy Adhesive
Thermal Transfer Composites PRIMEX ULTRA™ MCT-587™ Aluminum Silicon Carbide Composite, Reinforced
CeramTec Rocar® S Silicon Carbide, SSiC
Acerde Silicon Carbide
3M Techical Ceramics Ekasic® P Silicon Carbide

PEPOXY812 / 150837

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.