Notes: 66GF8 is a 40% glass fiber reinforced nylon 66 that offers excellent mechanical performance coupled with good surface finish and flow. Availability: Europe Fillers/Reinforcement: Glass Fiber, 40% Filler by Weight Features: Good Flow; Good Surface Finish Processing Method: Injection Molding Information provided by Teknor Apex |