Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X ASTM designation: PPA, polyphthalamide The main distinguishing features of Grivory HT, when compared to other polyamides, are its good performance at high temperatures providing parts, which are stiffer, stronger, have better heat distortion and dimensional stability as well as excellent chemical resistance and low moisture absorption. Grivory XE 4164 black 9225 is especially suitable for injection molded components in electrical and electronic applications. The material is suitable for lead-free SMT reflow soldering e.g. JEDEC J-STD-020C (peak temperature 260°C). Components conforming to JEDEC MSL1 are achievable.Information provided by EMS Grivory |