MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BNZ Materials Bazelite 2600 LI Insulating Castable
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Blazelite 2600 LI is s low iron, high purity castable for service to 2600°F (1427°C) in controlled atmosphere applications. Recommended for casting monolithic shapes and furnace linings

Information provided by BNZ Materials Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 72.0 lb/ft³Fired at 5 hrs at 816°C
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000690 GPa
@Temperature 1260 °C
ASTM C268
 0.000760 GPa
@Temperature 815 °C
ASTM C268
 0.000830 GPa
@Temperature 1095 °C
ASTM C268
 0.00110 GPa
@Temperature 540 °C
Fired; ASTM C268
 0.00165 GPa
@Temperature 104 °C
Dried; ASTM C268
 0.00207 GPa
@Temperature 1371 °C
ASTM C268
Compressive Strength 700 psi
@Temperature 815 °C
Cold Crush Strength
 700 psi
@Temperature 1095 °C
Cold Crush Strength
 700 psi
@Temperature 1260 °C
Cold Crush Strength
 700 psi
@Temperature 1371 °C
Cold Crush Strength
 700 psi
@Treatment Temp. 104 °C
Cold Crush Strength; Dried 104°C
 1000 psi
@Treatment Temp. 540 °C
Cold Crush Strength; Dried 104°C
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1427 °C
Shrinkage 0.20 %
@Temperature 540 °C
Permanent Linear Change; ASTM C210
 0.20 %
@Temperature 815 °C
Permanent Linear Change; ASTM C210
 0.20 %
@Temperature 1095 °C
Permanent Linear Change; ASTM C210
 0.50 %
@Temperature 1260 °C
Permanent Linear Change; ASTM C210
 2.1 %
@Temperature 1371 °C
Permanent Linear Change; ASTM C210
 
Component Elements PropertiesOriginal ValueComments
Al2O3 51 %
CaO 4.7 %
Fe2O3 0.80 %
MgO 0.10 %
Na2O 0.10 %Includes K2O
SiO2 40.1 %
TiO2 1.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silver Vanadium Oxide Fluoride, Ag4V2O6F2
Dow 1500 Antifoam
Sinotek Materials 3rd Class Carbon Rod for Dry Battery
Magnesium Elektron Melmag® AP65 Magnesium Alloy Battery Plate Rod Composition
Lithium, Li

CBNZ947 / 149187

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.