MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Teknor Apex Sarlink® TPE FM-2669 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Sarlink FM-2669 is a general purpose thermoplastic elastomer, available in Nat, Blk, and colors, used in a variety of automotive interior applications, including automotive floor mats. Sarlink FM-2669 is a UV stabilized, medium hardness, high density, wear-resistant grade suitable for extrusion, injection molding or thermoforming.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Filled; Good Adhesion; Good Colorability; Good Processability; Good Toughness; High Density; Medium Hardness; High Specific Gravity; Low Flow; UV Resistant; Wear Resistant

Uses: Automotive Applications; Automotive Interior Parts; Rubber Replacement

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding; Extrusion; Thermoforming

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 g/cc0.0415 lb/in³ISO 1183
Melt Flow 0.10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
0.10 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  74
@Time 15.0 sec
74
@Time 0.00417 hour
Injection Molded; ISO 868
 75
@Time 5.00 sec
75
@Time 0.00139 hour
Injection Molded; ISO 868
 79
@Time 1.00 sec
79
@Time 0.000278 hour
Injection Molded; ISO 868
Tensile Strength at Break 6.00 MPa870 psiISO 37
Elongation at Break 500 %500 %ISO 37
 
Processing PropertiesMetricEnglishComments
Processing Temperature 227 - 249 °C440 - 480 °FMelt, Injection
Rear Barrel Temperature 227 - 249 °C440 - 480 °FInjection
Middle Barrel Temperature 227 - 249 °C440 - 480 °FInjection
Front Barrel Temperature 227 - 249 °C440 - 480 °FInjection
Nozzle Temperature 227 - 249 °C440 - 480 °FInjection
Zone 1 216 - 238 °C420 - 460 °FExtrusion
Zone 2 216 - 238 °C420 - 460 °FExtrusion
Zone 3 216 - 238 °C420 - 460 °FExtrusion
Zone 4 216 - 238 °C420 - 460 °FExtrusion
Zone 5 216 - 238 °C420 - 460 °FExtrusion
Die Temperature 216 - 238 °C420 - 460 °FExtrusion
Mold Temperature 15.6 - 32.2 °C60.0 - 90.0 °FInjection
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiInjection
Back Pressure 0.172 - 0.862 MPa25.0 - 125 psiInjection
Cushion 0.381 - 2.54 cm0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 120 rpm50 - 120 rpmInjection
 
Descriptive Properties
AppearanceBlack
 Colors Available
 Natural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1047 / 237538

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.