MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil HD Plus 80W-90
Categories: Fluid; Lubricant

Material Notes: Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for performance in heavy-duty commercial transmissions, axles, and final drives where extreme pressures and shock loading are expected. They provide excellent chemical and thermal stability at elevated bulk oil temperatures, good performance at low temperatures, and have demonstrated good rust protection resulting from water contamination and wet conditions. They provide excellent performance where API GL-5 and MT-1 service is required.

Heavy-duty manual transmissions, axles, and final drives requiring API GL-5 and MT-1 level performance; On-highway light and heavy-duty trucks, busses, vans, and cars; Off-highway industries including: construction, mining, quarrying, and agriculture; Other heavy-duty industrial and automotive applications involving hypoid and other gears operating under conditions where high speed/shock load, high speed/low torque, and/or low speed/high torque conditions prevail; Mobilube HD Plus gear lubricants are intended for initial fill, top-off, and refill of enclosed commercial gearing in manual or semiautomatic transmissions where gear lubricants are recommended including drive axles and final drives; Not recommended for applications requiring API GL-4 Level performance; Not intended for transmissions for which engine oil or automatic transmission fluids are recommended

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.895 g/cc
@Temperature 15.0 °C
0.0323 lb/in³
@Temperature 59.0 °F
ASTM D4052
Viscosity Measurement 103103Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 139 cSt139 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 14.5 cSt14.5 cStASTM D445
 
Thermal PropertiesMetricEnglishComments
Pour Point -27.0 °C-16.6 °FASTM D97
Flash Point 210 °C410 °FASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WEXXON057 / 75482

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.