MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL GTX RNX130 PPE+PS+PA  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO; Polystyrene (PS)

Material Notes: 30% glass reinforced PPE+PS+PA alloy for automotive and nonautomotive applications. Recycle grade in black/gray only.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.33 g/cc1.33 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 138 MPa20000 psiType I, 5 mm/min; ASTM D638
Tensile Strength, Yield 138 MPa20000 psiType I, 5 mm/min; ASTM D638
Elongation at Break 5.0 %5.0 %Type I, 5 mm/min; ASTM D638
Elongation at Yield 5.0 %5.0 %Type I, 5 mm/min; ASTM D638
Flexural Strength 186 MPa27000 psi1.3 mm/min, 50 mm span; ASTM D790
 186 MPa27000 psi2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 7.86 GPa1140 ksi2.6 mm/min, 100 mm span; ASTM D790
 8.13 GPa1180 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 0.420 J/cm0.787 ft-lb/inASTM D256
Izod Impact, Unnotched 5.34 J/cm10.0 ft-lb/inASTM D4812
Dart Drop, Total Energy 6.00 J
@Temperature 23.0 °C
4.43 ft-lb
@Temperature 73.4 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 251 °C
@Thickness 3.20 mm
484 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 229 °C
@Thickness 3.20 mm
444 °F
@Thickness 0.126 in
unannealed; ASTM D648

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI52747 / 152793

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.